The Quality Prediction result indicates that this area of the part can have quality problems. The cooling time at the point you selected is too high for the material you chose.
The cooling time is one factor used to determine the Quality Prediction result. The Quality Prediction result is yellow or red in areas where the cooling time is too high.
The Quality Prediction result calculates relative cooling times. It only warns if an area has a high cooling time relative to the other parts of the model.
If a part has a yellow or red Quality Prediction result, find out why. If it is due to high cooling time, try making some of the changes recommended here.
If the part is mostly green with some small yellow areas, it can be acceptable. However, carefully examine the other result displays to see exactly how and where the results went wrong.
Warping occurs if the cooling time in one area of the model is much greater than in other areas.
It is best if the areas requiring the longest cooling time are at or near the gate.
To reduce excessive cycle time:
Each option requires individual consideration about all relevant aspects of the mold design specification.