During static loading, metric units
Jointed Material |
Solder Type |
Tension |
Shear |
R m [MPa] |
R ms [MPa] |
||
Low strength steels (for example, 37 grade) |
Tin solders |
30 to 80 |
20 to 40 |
Solders from Cu alloys |
200 to 350 |
100 to 220 |
|
Silver solders |
220 to 400 |
120 to 2520 |
During static loading, English units
Jointed Material |
Solder Type |
Tension |
Shear |
R m [psi] |
R ms [psi] |
||
Low strength steels (for example, 37 grade) |
Tin solders |
4 500 to 11 500 |
2 900 to 5 800 |
Solders from Cu alloys |
29 000 to 50 000 |
14 500 to 32 000 |
|
Silver solders |
32 000 to 58 000 |
17 500 to 36 000 |