Runner cross-sections - Shape

The shape of the runner affects the volume of material that remains molten.

Effects of shape

The cross-sectional shape of the runners affects the flow of the polymer through the runner system. When the hot melt hits the cold metal of the runner a layer freezes and forms a skin on the surface of the runner. The center of the runner remains molten while the polymer is being injected into the mold. The following diagram shows the molten center of different runner shapes.



A circular cross section provides the greatest proportion of polymer in a molten state. Runners with a curved or angular cross section require less force to remove from the mold than rectangular or square runners.

Although circular runners are the best choice for material flow and ejection, they are also the most expensive. This is partly because the runner needs to be cut into both plates and it is difficult to cut both halves of the runner so that they meet exactly.

A trapezoidal cross section can be used as a compromise. Trapezoidal runners often provide acceptable flow and ejection characteristics, and are cheaper to produce than round runners.

If you do use a circular runner, extra care is needed to align the two halves of the circular runner to avoid an increase in injection pressure due to the reduced effective flow cross-section. In the following diagram, the runner on the left is correctly aligned, but the runner on the right will have a smaller molten center that will restrict flow.


Mold alignment